Gail Kendall Clear (Blue)

Gail Kendall Clear (Blue)

Firing temperature : cone 04-03 | Surface texture : satin to glossy | Color : blue | Atmosphere: Oxidation/Neutral Reduction

This recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

The recipe above will produce a blue glaze. For a clear glaze, omit the Cobalt Carbonate and the Copper Oxide.

Since this recipe contains a high percentage of Gerstley borate, it is best to mix small batches that you will use relatively quickly, as the glaze will gel over time.