Firing temperature : cone 04 | Surface texture : glossy | Color : amber | Atmosphere: Oxidation/Neutral Reduction

This glaze is food safe and translucent. Test in Your own kiln with your materials and firing schedule to determine food safety, as results may be different.

Published in "Low-Fire Surfaces" by Ronan Kyle Peterson, in the September 2017 issue of Ceramics Monthly.