Firing temperature : cone 06-03 | Surface texture : matte | Color : white | Atmosphere: Oxidation/Neutral

Published in "Low-Fire Layering Glazes" by Matt Wedel, in the March 2014 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Fat White is a very finicky glaze. It settles very fast and can be known to crawl if not applied and fired correctly. When applied thick and on the appropriate surface, it can take on a foamy quality.