Firing temperature : cone 03-04 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

Adding CMC Gum makes this glaze easy to brush.

This recipe was shared by Kari Radasch in the March 2019 issue of Ceramics Monthly.