Firing temperature : cone 04 | Surface texture : glossy | Color : medium yellow | Atmosphere: Oxidation/Neutral

This is a shiny, transparent glaze that is very responsive to colorants. Without colorants, it is food safe. With colorants, you'll need to have it tested for leaching those colorants.

Published in "Polychrome Glazes" by Joan Bruneau, in the April 2014 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Apply thin in order to ensure the fired glaze will be a transparent clear. Use a thicker application with colorants to achieve a rich translucent glaze. Use 2–6% Mason stain.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend