Cushing Satin Matt

Cushing Satin Matt

Firing temperature : cone 4 | Surface texture : satin matte | Color : clear | Atmosphere: Oxidation/Neutral Reduction

Shown here on work by Paul Eshelman.

Published in "Val Cushing's Glazes" in the April 2014 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This glaze can be colored with oxides or stains, and 0.3% granular manganese dioxide added for speckles.