Instructions

The source of this recipe is unknown. Apply a thin coat for best results. Use a dry finger to smooth any pinhole-like marks on the surface before firing. This stable glaze has a softer shine than the high-gloss found in many clear glazes. I fire it to cone 1 with a 10-minute hold in an electric kiln.

This recipe was shared by Susan McHenry in the September 2019 issue of Ceramics Monthly.

 