Ceramic Recipes logo

Clear Glaze

Firing temperature : cone 04 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/Neutral

Published in "Low-Fire Glazes" by Lauren Karle, in the October 2016 issue of Ceramics Monthly.

Low-fire, clear glaze. Shown in the image here over a number of different slips and washes.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

To make this a brushable glaze, add CMC gum. Add a spoonful of the dissolved CMC gum into the glaze at a time. Test brushability and add one spoonful more at a time if necessary.

For better pouring, add an Epsom salts and water mixture. Slowly pour a small amount into the glaze and mix well. This will flocculate the glaze, making it dry quicker and prevent running and drips. It also prevents it from settling in the bucket. Dip or pour to test, adding more Epsom Salts if necessary.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend