Clear Base Glaze 2
Firing temperature : cone 03 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/NeutralPublished in " A Dialogue with Lisa Orr" by Rafael Molina-Rodriguez, in the May 2000 issue of Ceramics Monthly.
Ingredients