Chris Clear

Chris Clear

Firing temperature : cone 01-05 | Surface texture : glossy | Color : blue | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This glaze recipe originally came from a workshop with Lisa Orr.

This recipe was shared by Lorraine Olderman in the July/August 2019 issue of Pottery Making Illustrated.