Bright Glaze II
Firing temperature : cone 06 | Surface texture : matte | Color : dark red | Atmosphere: Oxidation/NeutralPublished in "Richard Behrens: A Tribute" by Tom Buck, in the Mar 2001 issue of Ceramics Monthly.