Bright Glaze II (turquoise)
Firing temperature : cone 06 | Surface texture : matte | Color : turquoise blue | Atmosphere: Oxidation/NeutralPublished in "Low-fire Alkaline Glazes" by Cheryl Pannabecker, in the May/June 2011 issue of Pottery Making Illustrated.
Ingredients
- 7.7
- 40.7