Borax Wash

Borax Wash

Firing temperature : cone 04-6 | Surface texture : satin | Color : clear | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Use hot water to dissolve the borax. It will recrystallize as it cools; this is fine, the crystals give a speckled effect.

This recipe was shared by Marty Fielding in the in the December 2020 issue of Ceramics Monthly.