Blue Low-Fire Glaze

Blue Low-Fire Glaze

Firing temperature : cone 04 | Surface texture : glossy | Color : blue | Atmosphere: Oxidation/Neutral Reduction

Click Image to Enlarge

Instructions

*Substitute Minspar 200 Feldspar for Kona F4 Feldspar, which is no longer mined. The glaze works well when sprayed or brushed on. For the best coverage, apply three coats whether spraying or brushing on the glaze.