Ceramic Recipes logo

Bill’s Basic Liner Glaze

Bill's Basic Liner Glaze

Firing temperature : cone 04-2 | Surface texture : glossy | Color : white | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

Use less zircopax for a less-opaque-white liner glaze. I use only 10%.

Substitute Minspar 200 for the Kona F-4 feldspar.

This recipe was shared by Adero Willard in the September/October 2014 issue of Pottery Making Illustrated.

 