Ceramic Recipes logo

Base Glaze – Aquamarine

Base Glaze – Aquamarine

Firing temperature : cone 04-03 | Surface texture : glossy | Color : blue green | Atmosphere: Oxidation/Neutral

Published in "Unity, Form, and Surface: A New Approach to Fritware" by Frank Krevens, in the Sep 2015 issue of Ceramics Monthly.

A fritted glaze developed to fit White Fritware clay body. Glossy glaze that breaks well over sharp edges. The glaze in the image shown here was fired to cone 04 with a 30-minute hold at peak temperature.


Click Image to Enlarge

Instructions

Mix all ingredients prior to adding the water.
.