Yellow

Firing temperature : cone 10 | Surface texture : matte to satin | Color : yellow | Atmosphere: Reduction Soda

Published in "Atmospheric Recipes," in the October 2018 issue of Ceramics Monthly. This recipe has been contributed by Stephen Heywood.


Click Image to Enlarge

Ingredients

Instructions

This glaze is not food safe. A thick application works best.