Ceramic Recipes logo

Yellow Speckle Glaze

Yellow Speckle Glaze

Firing temperature : cone 10 | Surface texture : satin matte | Color : dark yellow | Atmosphere: Reduction

Published in "A Typical Firing" by Alan Myers, in the May 2000 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Light Blue-Gray: add 20 grams red iron oxide

Light Green: add 80 grams red iron oxide

Dark Green: add 200 grams red iron oxide

Saturated Iron (Black): add 320 grams red iron oxide

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.