Firing temperature : cone 10 | Surface texture : matte to satin | Color : yellow | Atmosphere: Salt Soda

Published in "Yellow Flashing Slip," in the October 2018 issue of Ceramics Monthly. This recipe has been used by Stephen Heywood.


Click Image to Enlarge

Ingredients

Instructions

Apply a thin coat on dry greenware or bisqueware by dipping, pouring, spraying, or brushing. Ranges in color from dark mustard yellow to bright intense yellow depending on the clay body it is applied to.