Ceramic Recipes logo

Yellow Crystal Matte Glaze

Yellow Crystal Matte Glaze

Firing temperature : cone 8-11 | Surface texture : matte | Color : dark yellow | Atmosphere: Reduction

Published in "Tom and Elaine Coleman" by John Nance, in the Jan 2003 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This image shows Yellow Crystal Matt and Black Barium Matt Glazes with dry mesquite ash sprinkled on top.

For use on exterior or decorative surfaces. Yields a beautiful butter-smooth glaze that develops crystals. For a yellow-gold, add 2% yellow iron oxide. Responsive to oxide oversprays. For a pumpkin orange, spray with Spotted Black Glaze.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend