Woo White
Firing temperature : cone 10 | Surface texture : matte | Color : white | Atmosphere: Oxidation/Neutral ReductionPublished in "Modernist Series" in the Nov 2014 issue of Ceramics Monthly.
Ingredients
- 25
- 12
- 34
- 7
- 7
Instructions
Fires to an opaque matte surface. Works will in oxidation or reduction. Good in salt/soda firings. This glaze is not food safe.