Wild Rose
Firing temperature : cone 6-9 | Surface texture : glossy | Color : dark brown | Atmosphere: ReductionPublished in "Modernist Series" in the Nov 2014 issue of Ceramics Monthly.
Ingredients
- 10
- 10
- 62
Instructions
Tenmoku-like brown/black, but super shiny and sometimes gold metallic.