Virden Wrinkle (Black)

Virden Wrinkle (Black)

Firing temperature : cone 10 | Surface texture : glossy to satin | Color : black | Atmosphere: Reduction

Click Image to Enlarge

Instructions

I like using this glaze for its softness. It is a nice matte black with a lot of variety in the surface it produces. I’ve dipped pots in this glaze, but get the best results when it’s sprayed until a heavy dusting is applied to the pot. Be careful not to apply too thick because it will crack off. In light reduction, the surface will be more uniform, but a heavier reduction will provide more texture and movement.

This recipe was shared by Antonio Martinez in the September 2020 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend