VC Amber Celadon
Firing temperature : cone 9-11 | Surface texture : glossy | Color : amber | Atmosphere: ReductionIngredients
- 2.04
- 3.06
- 14.30
- 9.18
- 19.39
- 10.20
- 2.04
- 29.59
Instructions
Apply glaze about a fingernail thickness on the surface. This glaze moves a lot when fired hotter than cone 10. Wax at least ¼ inch up from the foot ring.
This recipe was shared by Andrew McIntyre in the April 2019 issue of Ceramics Monthly.