Turquoise Lorios

Turquoise Lorios

Firing temperature : cone 10 | Surface texture : satin matte | Color : medium green | Atmosphere: Oxidation/Neutral

This glaze is from Sally Brogden (University of Tennessee).

The test tile is Coleman Porcelain fired in oxidation.

The glaze is reddish-pink when fired in reduction.


Click Image to Enlarge

Ingredients

Instructions

Can be runny if applied thickly.