Firing temperature : cone 10 | Surface texture : satin matte | Color : clear | Atmosphere: Oxidation/Neutral Reduction

Published in "Cone 10 Transparent" by Antoinette Badenhorst, in the June 2015 issue of Ceramics Monthly.

A transparent base glaze that can be used as a clear or with colorants. Fire to cone 10 for a stain finish. Try testing up to 10% commercial stains for different colors.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Mix all ingredients together prior to adding the water. Adding a small amount of valium chloride helps keep the glaze in suspension.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend