Titanium White

Firing temperature : cone 10-11 | Surface texture : glossy to satin | Color : white | Atmosphere: Reduction Soda

This recipe was shared in the January 2019 issue of Ceramics Monthly by Adrian King.


Click Image to Enlarge

Ingredients

Instructions

Apply to a medium thickness. This glaze will run when hot as well as when layered with other glazes. I soda fire this glaze to cone 10–11 reduction in a gas-fired kiln.