Firing temperature : cone 10-11 | Surface texture : glossy | Color : Tenmoku | Atmosphere: Oxidation Reduction Soda

This recipe was shared in the January 2019 issue of Ceramics Monthly by Adrian King.


Click Image to Enlarge

Ingredients

Instructions

Apply a medium thickness to show slips through the glaze. A heavier reduction atmosphere results in a more red/black glaze. A more oxidized atmosphere produces a yellow/black glaze. I soda fire this glaze to cone 10–11 reduction in a gas-fired kiln.