Ceramic Recipes logo

Temple Black

Temple Black

Firing temperature : cone 10 | Surface texture : glossy to satin | Color : black | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

I use Mason Stain (MS) Best Black, but other colorants may work with testing. Applied thin it resembles gun metal, applied thick it's a semi-matte charcoal. Stir frequently or add bentonite.

This recipe was shared by Seth Guzovksy in the January/February 2020 issue of Pottery Making Illustrated.