Firing temperature : cone 10 | Surface texture : satin matte | Color : cream | Atmosphere: Oxidation/Neutral

This is a version of a Steven Hill glaze. The test tile is B-Mix, fired in oxidation.


Click Image to Enlarge

Instructions

This glaze can be runny if applied thickly.