Firing temperature : cone 10-11 | Surface texture : glossy to satin | Color : brown | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Once pots are decorated with Hannah’s Fake Ash glaze, I then dip them in this glaze, which I mix to the consistency of heavy cream. It must be fired hot, to cone 10–11 in moderate to heavy reduction starting at cone 012.

This recipe was shared by Terry Plasket in the June/July/August 2021 issue of Ceramics Monthly.