Firing temperature : cone 10 | Surface texture : satin | Color : white | Atmosphere: Reduction

Click Image to Enlarge

Instructions

Add enough water to make the glaze slurry a thick cream consistency. Sieve with an 80-mesh screen prior to use.

This recipe was shared by Natasha Alphonse in the June/July/August 2021 issue of Ceramics Monthly.