SG-302 Opaque Gray-Tan Matte with Whiting
Firing temperature : cone 10 | Surface texture : satin matte | Color : medium tan | Atmosphere: Oxidation/Neutral ReductionPublished in "Strontium/Barium" by Dave Finkelnburg, in the Nov 2014 issue of Ceramics Monthly.