Ceramic Recipes logo

Seth’s Gold

Seth’s Gold

Firing temperature : cone 10 | Surface texture : matte | Color : gold | Atmosphere: Oxidation/Neutral Reduction

This recipe is based on a glaze originally named "Reynold's Gold".

Not food safe.  Handle with care. Fire with proper ventilation. Good in reduction or oxidation.


Click Image to Enlarge

Instructions

Can be runny if applied thickly.