Ceramic Recipes logo

San Miguel Icy Blue

San Miguel Icy Blue

Firing temperature : cone 10 | Surface texture : glossy | Color : blue | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

Fire in oxidation for a glossy clear.

This recipe was shared by Mark Chuck in the June/July/August 2019 issue of Ceramics Monthly.