Sam Chung’s Satin Mint

Firing temperature : cone 10 | Surface texture : satin | Color : light green | Atmosphere: Oxidation/Neutral

Published in "Cone 10 Glazes" by Holly Hanessian, in the Feb 2017 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Substitute Minspar 200 Feldspar for the Kona F-4 Feldspar. This glaze works best when applied quite thinly. When surrounded by tiles glazed with John Britt's Nickel Yellow glaze during the firing, the Sam Chung's Satin Mint changed slightly in color.