Ceramic Recipes logo

Rutile Blue

Rutile Blue

Firing temperature : cone 10 | Surface texture : glossy | Color : blue | Atmosphere: Reduction

Published in "Rutile" by Ryan Coppage, in the October 2017 issue of Ceramics Monthly.


Click Image to Enlarge

Ingredients

Instructions

This glaze is great when with a tenmoku glaze over it, but not vice versa.