Rutile Base

Firing temperature : cone 10 | Surface texture : glossy | Color : blue | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

To get the rivulets shown in image 3, apply Red- Black Glaze and Mel’s Orange Underglaze, then lay- er over the top half of the piece with any rutile base from Glazy.org, such as the recipe shown above.

This recipe was shared by Mark Cortright in the October 2021 issue of Ceramics Monthly.