Ceramic Recipes logo

Ron Roy Base—Silver Nitrate

Ron Roy Base—Silver Nitrate

Firing temperature : cone 10 | Color : brown | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

This recipe can be fired to cone 6 in oxidation (left tile) and cone 10 in reduction (right tile).

To achieve good color results, thicker application is better, as this glaze is incredibly stable and does not run much. If firing in oxidation, a medium firing ramp with a 15-minute hold at the top temperature is sufficient to let any off-gassing pinholes seal over.

This recipe was shared by Ryan Coppage in the October 2021 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend