Red-Black Glaze

Red-Black Glaze

Firing temperature : cone 10 | Surface texture : glossy | Color : black | Atmosphere: Reduction

Click Image to Enlarge

Instructions

Only a quick dip is needed to apply this glaze as it will run if applied too thick. Fire this glaze to cone 10 in reduction in a gas kiln.

This recipe was shared by Mark Cortright in the October 2021 issue of Ceramics Monthly.