Ceramic Recipes logo

Pinnell Celadon

Pinnell Celadon

Firing temperature : cone 10 | Surface texture : matte | Color : pink | Atmosphere: Reduction

Published in "Copper Oxide" by John Britt, in the Jun 2012 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Celadon glaze with tin oxide, pink flashing of copper from Oribe glazed pieces next to it in the kiln.