Pete’s Weathered Bronze

Pete's Weathered Bronze

Firing temperature : cone 6-9 | Surface texture : satin | Color : bronze | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

This greenish glaze has a wide firing range. It is more bronze-like in coloration and depth at cone 9 in reduction. This glaze breaks on the edges and pools in recesses. Attributed to Pete Pinnell.

This recipe was shared Eve Behar in the July/August 2021 issue of Pottery Making Illustrated.