Pete’s STD Shino

Firing temperature : cone 10 | Surface texture : glossy | Color : various | Atmosphere: Reduction

Found in 2005 Shino Review

Single-dipped renders a light red choral color.

Double-dipped renders a light pastel lavender color


Click Image to Enlarge

Instructions

Mixed by hand with equal weight in water as ingredients, then dipped (single and double pictured)