Ceramic Recipes logo

Peggy’s Oribe Glaze

Peggy’s Oribe Glaze

Firing temperature : cone 11 | Surface texture : matte | Color : medium brown | Atmosphere: Reduction

Published in "Firing the Hikarigama" by Janet Buskirk, in the Apr 2001 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions