Firing temperature : cone 10 | Surface texture : glossy | Color : shino | Atmosphere: Reduction

Click Image to Enlarge

Instructions

I fire this glaze up to cone 11–12 in heavy reduction in a wood kiln, but it is also suitable for firing in a gas kiln to cone 10 in normal reduction.

This recipe was shared by Monte Young in the March 2020 issue of Ceramics Monthly.