Oribe Green

Firing temperature : cone 10 | Surface texture : glossy | Color : blue | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

I fire this glaze up to cone 11–12 on heavy reduction in a wood kiln, but it also works fine fired in a gas kiln to cone 10 in normal reduction.

This recipe was shared by Monte Young in the March 2020 issue of Ceramics Monthly.