Firing temperature : cone 10 | Surface texture : satin matte | Color : medium orange | Atmosphere: Reduction

Published in "Exploring Glazes: From Perfect fit to Crackle and Matte," in the March 2016 issue of Ceramics Monthly.

The lithium in this glaze activates the surface and makes this glaze work.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Use at a specific gravity of 1.4 or 1.42. When the glaze is applied at that proper thickness, the surface crackles as it dries. If applied too thick, it will crack off.