Orange Crush Glaze

Firing temperature : cone 9 | Surface texture : satin matte | Color : Orange | Atmosphere: Oxidation

This recipe was shared by Ernest Miller is the January/February 2019 issue of Pottery Making Illustrated.


Click Image to Enlarge

Ingredients

Instructions

This glaze fires bright orange on white clay while firing dark orange-brown on an iron-bearing clay.