Firing temperature : cone 10 | Surface texture : glossy | Color : brown | Atmosphere: Reduction Salt Soda

Click Image to Enlarge

Ingredients

Instructions

This is a very rich warm brown with red hues that run through it. I use this as a liner glaze for most of my pagoda vessels. I like the contrast of dark to light with the flashes of orange, gold, red, and white that the salt/soda firings give me.

This recipe was shared by Arylnn Nobel in the May/June 2021 issue of Pottery Making Illustrated.