Firing temperature : cone 10 | Surface texture : glossy | Color : various | Atmosphere: Reduction

Burnt orange shino when single dipped, greyish-white when applied thicker. (fired at cone 9-11)  Some crazing occurs when thickly applied.

Source: American Shino (Book) - Jeff Oestreich


Click Image to Enlarge

Instructions

Test batch was mixed by hand.  Test tile dipped fully once and half-dipped a second time.